The first stage of expansion is the addition of a flotation circuit that includes a regrind mill for processing flotation concentrate to approximately P80 20 microns prior to feeding the pre ...
The first stage of expansion is the addition of a flotation circuit that includes a regrind mill for processing flotation concentrate to approximately P80 20 microns prior to feeding the pre ...
Applying a 350 micron ("µm") primary grind with CPF scavenging returns comparable copper recovery to a conventional flotation circuit with a 200 µm primary grind 3. Significant increase to mill ...
North Vancouver, British Columbia--(Newsfile Corp. - March 20, 2025) - Lion One Metals Limited (TSXV: LIO) (OTCQX: LOMLF) ("Lion One" or the "Company") is pleased to announce the start of engineering ...